Dafnelen®
Homopolymer- und Copolymer-Polypropylen-Compounds mit hohen mechanischen Eigenschaften, die in Übereinstimmung mit den Marktanforderungen und Industriestandards entwickelt wurden. Die Produkte sind in einer breiten Farbpalette und in zertifizierten flammhemmenden Versionen erhältlich, sowohl halogenhaltig als auch halogenfrei.Name | Compound | MFR ISO 1133 | MFR (g/10’) ASTM D1238 | Biegemodul ISO 178 | MFR (g/10’) ASTM D1238 | Izod Gekerbt ISO 180/1A | Izod Gekerbt ASTM D256 | Entflammbarkeit UL94/2 | |
---|---|---|---|---|---|---|---|---|---|
Dafnelen® CR 09/K | PP copo flame retardant halogen free UL94 V0 (0,8mm) | 10 g/10' | - | 1900 MPa | - | 3,5 Kj/m2 | - | Classe V0-5VA YC | |
Dafnelen® HP 1003/S | 50% glass fibers chemical grafting. | 3 g/10' | - | 10500 Mpa | - | 12 KJ/m2 | - | Classe HB | |
Dafnelen® HP 505/SW | PP homo 25% glass fiber, flame retardant V0 | 5 g/10' | - | 6500 MPa | - | 6 Kj/m2 | - | Classe V0 | |
Dafnelen® HP 605/SW | PP homo 30% glass fiber, flame retardant V0 | 4 g/10' | - | 8000 MPa | - | 7 Kj/m2 | - | Classe V0 YC | |
Dafnelen® HR 17/Y | Unfilled homopolymer polypropylene.Flame Retardant grade Halogen-free according to IEC 61249-2-21 | 17 g/10' | - | 1500 Mpa | - | 5 KJ/m2 | - | Classe V2 |
Dafneglass®
Glasfaserverstärktes Verbundpolypropylen, chemisch oder mechanisch gebunden, mit hohen thermischen Eigenschaften, exzellenter Schlagzähigkeit und Steifigkeit, gemäß den Standards der Automobil- und Haushaltsgeräteindustrie.Die Produkte sind in den für die jeweiligen Branchen vorgegebenen Farben und selbstverlöschenden Versionen, auch halogenfrei erhältlich.
Name | Compound | MFR ISO 1133 | MFR (g/10’) ASTM D1238 | Biegemodul ISO 178 | MFR (g/10’) ASTM D1238 | Izod Gekerbt ISO 180/1A | Izod Gekerbt ASTM D256 | Entflammbarkeit UL94/2 | |
---|---|---|---|---|---|---|---|---|---|
Dafneglass® HP 505/K | PP homo 25% glass fiber, flame retardant grade without halogens, heat stabilized. | 3,5 g/10' | - | 7000 MPa | - | 7,3 Kj/m2 | - | Classe V0 | |
Dafneglass® HP 605/K | 30% chemically coupled glass fiber reinforced polypropylene. V0 flame retardant grade. Heat stabilized. Flame Retardant grade Without halogens. | 2 g/10' | - | 7600 Mpa | - | 8 KJ/m2 | - | Classe HB |
Isoplen®
Homopolymer- und Copolymer-Polypropylen-Compounds mit hohen mechanischen Eigenschaften, die in Übereinstimmung mit den Marktanforderungen und Industriestandards entwickelt wurden. Die Produkte sind in einer breiten Farbpalette und in zertifizierten flammhemmenden Versionen erhältlich, sowohl halogenhaltig als auch halogenfrei.Name | Compound | MFR ISO 1133 | MFR (g/10’) ASTM D1238 | Biegemodul ISO 178 | MFR (g/10’) ASTM D1238 | Izod Gekerbt ISO 180/1A | Izod Gekerbt ASTM D256 | Entflammbarkeit UL94/2 | |
---|---|---|---|---|---|---|---|---|---|
Isoplen® A H F | PP homo, natural colour medium flowability | 12 g/10' | - | 1400 MPa | - | 3,3 Kj/m2 | - | Classe HB | |
Isoplen® A K F | PP copo, medium flowability | 13 g/10' | - | 1300 MPa | - | 11 Kj/m2 | - | Classe HB | |
Isoplen® A K Z | PP copo, high flowability | 21 g/10' | - | 1350 MPa | - | 5,6 Kj/m2 | - | Classe HB | |
Isoplen® FR V2 | PP copo flame retardant low halogen content | 10 g/10' | - | 1400 MPa | - | 10 Kj/m2 | - | Classe V2 YC | |
Isoplen® H2 T V | PP homo, natural colour, heat stabilized, high flowability | 20 g/10' | - | 1400 MPa | - | 5 Kj/m2 | - | Classe HB | |
Isoplen® HK X V0 HF | Unfilled. Heat stabilized. Flame Retardant grade without halogens. | 10 g/10' | - | 1600 Mpa | - | 3,5 KJ/m2 | - | Classe V0 YC |
Isoflex®
Copolymer-Polypropylen, ungefüllt und nicht stabilisiert.Name | Compound | MFR ISO 1133 | MFR (g/10’) ASTM D1238 | Biegemodul ISO 178 | MFR (g/10’) ASTM D1238 | Izod Gekerbt ISO 180/1A | Izod Gekerbt ASTM D256 | Entflammbarkeit UL94/2 | |
---|---|---|---|---|---|---|---|---|---|
Isoflex® C800 | Polypropylene copolymer. | 6 g/10' | - | 800 Mpa | - | 45 KJ/m2 | - | / |
Isofil®
Standard- und High-Performance-modifiziertes Polypropylen mit verschiedenen mineralischen Füllstoffen (T/TC/CaCO3/BaSO4/Glimmer) in Übereinstimmung mit den Marktanforderungen und Industriestandards. Produkte mit Anwendungsmerkmalen in gemeinsam mit Kunden entwickelten Farben und Spezifikationen. Zertifizierte flammhemmende Versionen sind sowohl halogenhaltig als auch halogenfrei erhältlich.Name | Compound | MFR ISO 1133 | MFR (g/10’) ASTM D1238 | Biegemodul ISO 178 | MFR (g/10’) ASTM D1238 | Izod Gekerbt ISO 180/1A | Izod Gekerbt ASTM D256 | Entflammbarkeit UL94/2 | |
---|---|---|---|---|---|---|---|---|---|
Isofil® H 20 T F UV | 20% talc filled homopolymer polypropylene. UV stabilized. | 15 g/10' | - | 2600 Mpa | - | 2,5 KJ/m2 | - | Classe HB | |
Isofil® H 20 TP F HS | 20% Talc filled polypropylene homopolymer. Low emission. Compliant to VW44045-PP6.Heat stabilized. | 12 g/10' | - | 2800 Mpa | - | 3 KJ/m2 | - | Classe Hb | |
Isofil® H 20 TP X | PP homo 20% talc natural colour | 9 g/10' | - | 2600 MPa | - | 3 Kj/m2 | - | Classe HB | |
Isofil® H 40 C2 F | 40% calcium carbonate filled homopolymer polypropylene. | 13 g/10' | - | 2500 Mpa | - | 3,3 KJ/m2 | - | Classe HB YC | |
Isofil® H 40 C2 X | 40% calcite filled homopolymer polypropylene. | 9 g/10' | - | 2400 Mpa | - | 3,3 KJ/m2 | - | Classe HB YC | |
Isofil® H 40 TG S HS | 40% talc filled polypropylene homopolymer. | 10 kg/10' | - | 4100 Mpa | - | 3,5 KJ/m2 | - | Classe HB | |
Isofil® H 40 TG X HS | 40% talc filled homopolymer polypropylene. Compliant to VW 44045-PP8. Heat stabilized. | 15 g/10' | - | 4000 Mpa | - | 2,5 KJ/m2 | - | Classe HB | |
Isofil® H 40 TP F | PP homo 40% talc | 12 g/10' | - | 4000 MPa | - | 2,4 Kj/m2 | - | Classe HB | |
Isofil® HF 2206H L | 10% talc filled polypropylene copolymer. Heat stabilized. Laserable. | 12 g/10' | - | 1500 Mpa | - | 8 KJ/m2 | - | Classe HB | |
Isofil® HF 6205X | 30% talc filled copolymer polypropylene. UV stabilized. Heat stabilized. | 14 g/10' | - | 2300 Mpa | - | 6 KJ/m2 | - | Classe HB | |
Isofil® HK 10 TVHM | - | - | - | - | - | - | - | - | |
Isofil® HK 20 2VH0 | 20% calcium carbonate polypropylene. Heat stabilized. | 16 g/10' | - | 1850 Mpa | - | 2,4 KJ/m2 | - | Classe HB YC | |
Isofil® HK 20 T V0 | 20% talc filled copolymer polypropylene. Heat stabilized. Flame Retardant grade With halogens | 6 g/10' | - | 2900 Mpa | - | 3,5 KJ/m2 | - | Classe HB | |
Isofil® HK 20 TCH0 | 20% mineral filled polypropylene. Heast stabilized. | 6 g/10' | - | 2300 Mpa | - | 3,3 KJ/m2 | - | Classe HB YC | |
Isofil® HK 20 TFH0 | 20% mineral filled polypropylene. Heat stabilized. | 13 g/10' | - | 2300 Mpa | - | 3,3 KJ/m2 | - | Classe HB YC | |
Isofil® HK 20 TFHH | 20% talc filled polypropylene. Heat stabilized. Detergent Resistant. | 5 g/10' | - | 2200 Mpa | - | 3,9 KJ/m2 | - | Classe HB YC | |
Isofil® HK 20 TP F HS | 20% talc filled copolymer polypropylene. | 12 g/10' | - | 2200 Mpa | - | 6 KJ/m2 | - | Classe HB | |
Isofil® HK 25 6VH | 25% talc-calcium carbonate filled polypropylene. | 16 g/10' | - | 2400 Mpa | - | 5 KJ/m2 | - | Classe HB YC | |
Isofil® HK 25 GVH | 25% talc filled copolymer polypropylene. | 16 g/10' | - | 2200 Mpa | - | 5,1 KJ/m2 | - | Classe HB YC | |
Isofil® HK 25 GVH1 | 25% talc copolymer polypropylene. Heat stabilized. | 17 g/10' | - | 2000 Mpa | - | 12,9 KJ/m2 | - | Classe HB YC | |
Isofil® HK 25 TVH0 | 25% talc filled copolymer polypropylene. | 23 g/10' | - | 1800 Mpa | - | 7 KJ/m2 | - | Classe HB YC | |
Isofil® HK 30 TFH2 | 30% talc filled polypropylene. | 14 g/10' | - | 34600 Mpa | - | 3,8 KJ/m2 | - | Classe HB YC | |
Isofil® HK 30 TSH1 | 30% talc filled polypropylene homopolymer. Heat stabilized. | 3 g/10' | - | 3500 Mpa | - | 5 KJ/m2 | - | Classe HB YC | |
Isofil® HK 30 TTH0 | 30% talc polypropylene. | 4 g/10' | - | 3300 Mpa | - | 3,1 KJ/m2 | - | Classe HB YC | |
Isofil® HK 30 TTH1 | 30% talc filled polypropylene. UV stabilized. Heat stabilized. | 3 g/10' | - | 3400 Mpa | - | 2,3 KJ/m2 | - | Classe HB YC | |
Isofil® HK 30 TVH0 | 30% talc filled homopolymer polypropylene. | 20 g/10' | - | 3400 Mpa | - | 3,3 KJ/m2 | - | Classe HB YC | |
Isofil® HK 30 TVH2 | 30% talc filled polypropylene. | 16 g/10' | - | 3200 Mpa | - | 3,3 KJ/m2 | - | Classe HB YC | |
Isofil® HK 30 TXH0 | 30% talc filled polypropylene. Heat stabilized. | 8 g/10' | - | 3300 Mpa | - | 2,7 KJ/m2 | - | Classe HB YC | |
Isofil® HK 35 GVH0 | 35% talc filled copolymer polypropylene. | 21 g/10' | - | 3100 Mpa | - | 3,3 KJ/m2 | - | Classe HB YC | |
Isofil® HK 40 2FH0 | 40% calcium carbonate filled polypropylene. Heat stabilized. | 13 g/10' | - | 2500 Mpa | - | 3,3 KJ/m2 | - | Classe HB YC | |
Isofil® HK 40 5FH0 | 40% calcium carbonate polypropylene. | 13 g/10' | - | 2500 Mpa | - | 3,3 KJ/m2 | - | Classe HB YC | |
Isofil® HK 40 TTH0 | 40% talc filled homopolymer polypropylene. Heat stabilized. | 4 g/10' | - | 3800 Mpa | - | 2,4 KJ/m2 | - | Classe HB YC | |
Isofil® HK 40 TVH0 | 40% talc filled copolymer polypropylene. | 18 g/10' | - | 4000 Mpa | - | 3 KJ/m2 | - | Classe HB YC | |
Isofil® HK 50 2FH0 | 50% calcium carbonate filled polypropylene. | 20 g/10' | - | 2800 Mpa | - | 3,5 KJ/m2 | - | Classe HB | |
Isofil® HK 50 C2 V | 50% calcium carbonate homopolymer polypropylene. Heat stabilized. | 18 g/10' | - | 3100 Mpa | - | 2,5 KJ/m2 | - | Classe HB YC | |
Isofil® HZ 9101D | 40% talc filled homopolymer polypropylene. Good flowability. | 23 g/10' | - | 4100 Mpa | - | 2,5 KJ/m2 | - | Classe HB | |
Isofil® K 0 T xxx HB | Copolymer polypropylene. | 17 g/10' | - | 1200 Mpa | - | 7,9 KJ/m2 | - | Classe HB YC | |
Isofil® K 10 T 46.400 AFU | 10% talc filled copolymer polypropylene. Scratch resistant. UV stabilized. | 22 g/10' | - | 1300 Mpa | - | 40 KJ/m2 | - | Classe HB | |
Isofil® K 10 T 53.180U | 13% talc filled copolymer polypropylene. UV stabilized. Scratch Resistant. | 15 g/10' | - | 1650 Mpa | - | 18 KJ/m2 | - | Classe HB | |
Isofil® K 20 T 48.450 AFU | 20% talc filled copolymer polypropylene. Impact modified and scratch resistant. UV stabilized. | 19 g/10' | - | 1700 Mpa | - | 45 KJ/m2 | - | Classe HB | |
Isofil® K 20 T 50.400LCE SR AF | 17% talc filled copolymer polypropylene. Low CLTE and scratch resistant. UV stabilized. | 32 g/10' | - | 1450 Mpa | - | 40 KJ/m2 | - | Classe HB | |
Isofil® K 20 T xxx HB | 20% talc filled copolymer polypropylene. | 16 g/10' | - | 2300 Mpa | - | 6,5 KJ/m2 | - | Classe HB YC | |
Isofil® K 20 TP X | PP copo 20% talc | 10 g/10' | - | 2000 MPa | - | 7 Kj/m2 | - | Classe HB | |
Isofil® K 30 T 50.200LCE SR AF | 30% talc filled copolymer polypropylene. High impact. Scratch resistant. High fluidity. UV stabilized. | 33 g/10' | - | 1700 Mpa | - | 20 KJ/m2 | - | Classe HB | |
Isofil® K 30 T 60.90L | 30% talc filled copolymer polypropylene. UV stabilized. | 16 g/10' | - | 2300 Mpa | - | 9 KJ/m2 | - | Classe HB | |
Isofil® K 40 T | 40% talc filled polypropylene. | 7 g/10' | - | 4200 Mpa | - | 2,6 KJ/m2 | - | Classe HB | |
Isofil® K 40 T xxx HB | 40% talc filled copolymer polypropylene. Heat stabilized. | 8 g/10' | - | 3800 Mpa | - | 2,6 KJ/m2 | - | Classe HB YC | |
Isofil® K 40 TP V | PP copo 40% talc | 20 g/10' | - | 3400 MPa | - | 4,2 Kj/m2 | - | Classe HB | |
Isofil® KGF 4002U | 21,5% talc filled copolymer polypropylene. UV stabilized. | 12 g/10' | - | 2000 Mpa | - | 4 KJ/m2 | - | Classe HB | |
Isofil® KPZ 4001D | 20% talc filled copolymer polypropylene. Heat stabilized. | 20 g/10' | - | 2400 Mpa | - | 4,7 KJ/m2 | - | Classe HB YC | |
Isofil® MC 4214Y | 20% talc filled copolymer polypropylene. UV stabilized. Scratch Resistant. | 8 g/10' | - | 2300 Mpa | - | 7 KJ/m2 | - | Classe HB | |
Isofil® MF 3604Y | 16% talc filled polypropylene. Impact resistance grade. UV stabilized. Scratch Resistant. | 14 g/10' | - | 1500 Mpa | - | 30 KJ/m2 | - | Classe HB | |
Isofil® MF 4124S | 20% talc filled polypropylene compound. It exhibits high stiffness and low emission properties. Scratch Resistant. | 15 g/10' | - | 2700 Mpa | - | 4 KJ/m2 | - | Classe HB | |
Isofil® MV 4509Y | 20% talc filled polypropylene copolymer. Impact modified. UV stabilized. Scratch Resistant. | 26 g/10' | - | 1900 Mpa | - | 30 KJ/m2 | - | Classe HB | |
Isofil® MY 2205Y | 10% talc filled copolymer polypropylene. Low emission grade. Scratch Resistant. | 25 g/10' | - | 1600 Mpa | - | 18 KJ/m2 | - | Classe HB | |
Isofil® MZ 2102H | 10% talc filled homopolymer polypropylene. Low emission grade. | 25 g/10' | - | 2350 Mpa | - | 3,5 KJ/m2 | - | Classe HB | |
Isofil® MZ 3506Y | 17% talc filled copolymer polypropylene. Good flowability. Low emission. UV stabilized. Heat stabilized. Scratch Resistant. | 22 g/10' | - | 2000 Mpa | - | 25 KJ/m2 | - | Classe HB | |
Isofil® PF 4102H | 20% Talc filled polypropylene homopolymer. Low emission. Compliant to VW44045-PP6 and WSS-M4D729-B1. Heat stabilized. | 12 g/10' | - | 2800 Mpa | - | 3 KJ/m2 | - | Classe HB | |
Isofil® PZ 8103H | 40% talc filled polypropylene homopolymer. Heat stabilized. | 20 g/10' | - | 4300 Mpa | - | 3 KJ/m2 | - | Classe HB | |
Isofil® RF 3403Y | 15% talc filled polypropylene copolymer. Impact modified. High fluidity. Low CLTE. UV stabilized. Scratch Resistant. | 15 g/10' | - | 1700 Mpa | - | 25 KJ/m2 | - | Classe HB | |
Isofil® RV 4603S | 20% talc filled impact modified polypropylene. Compliant to TL 52388-F. UV stabilized. Scratch Resistant. | 18 g/10' | - | 2000 Mpa | - | 35 KJ/m2 | - | Classe HB | |
Isofil® SF 4303U | 20% talc filled copolymer polypropylene with good stiffness and impact resistance. UV stabilized. | 15 g/10' | - | 1800 Mpa | - | 15 KJ/m2 | - | Classe HB | |
Isofil® SF 4501Y | 20% talc filled copolymer polypropylene. Impact modified grade. UV stabilized. Scratch Resistant. | 14 g/10' | - | 1900 Mpa | - | 20 KJ/m2 | - | Classe HB | |
Isofil® SV 4118X | 20% talc filled homopolymer polypropylene. Compliant to TL 52658-WD01. UV stabilized. Heat stabilized. | 16 g/10' | - | 2800 Mpa | - | 2,5 KJ/m2 | - | Classe HB | |
Isofil® SV 4205Y | 20% talc filled polypropylene copolymer. Good flowability and stiffness. UV stabilized. Scratch Resistant. | 16 g/10' | - | 2300 Mpa | - | 6 KJ/m2 | - | Classe HB | |
Isofil® SW 4909U | 20% talc filled copolymer polypropylene. Impact modified grade with high flowability. UV stabilized. | 40 g/10' | - | 1500 Mpa | - | 40 KJ/m2 | - | Classe HB |
Isoglass®
Glasfaserverstärktes Verbundpolypropylen, chemisch oder mechanisch gebunden, mit hohen thermischen Eigenschaften, exzellenter Schlagzähigkeit und Steifigkeit, gemäß den Standards der Automobil- und Haushaltsgeräteindustrie.Die Produkte sind in den für die jeweiligen Branchen vorgegebenen Farben und selbstverlöschenden Versionen, auch halogenfrei erhältlich.
Name | Compound | MFR ISO 1133 | MFR (g/10’) ASTM D1238 | Biegemodul ISO 178 | MFR (g/10’) ASTM D1238 | Izod Gekerbt ISO 180/1A | Izod Gekerbt ASTM D256 | Entflammbarkeit UL94/2 | |
---|---|---|---|---|---|---|---|---|---|
Isoglass® 4F 4030U | 22% chemically coupled glass fiber and mineral filled reinforced polypropylene copolymer. Good stiffness and impact strenght balance combined with high flowability. UV stabilized. | 14 g/10' | - | 3200 Mpa | - | 9 KJ/m2 | - | Classe HB | |
Isoglass® EV 3007U | 15% chemically coupled glass fiber reinforced polypropylene copolymer. High flowability grade and good aesthetical appearance. UV stabilized. | 18 g/10' | - | 2600 Mpa | - | 12 KJ/m2 | - | Classe HB | |
Isoglass® H 20 CGF X | 20% glass fiber reinforced homopolymer polypropylene. | 8 g/10' | - | 3800 MPa | - | 8 Kj/m2 | - | Classe HB | |
Isoglass® H 20 CGF X HS | 20% chemically coupled glass fiber reinforced homopolymer polypropylene. Compliant to VW 44045-PP9. Heat stabilized. | 8 g/10' | - | 4000 Mpa | - | 7 KJ/m2 | - | Classe HB | |
Isoglass® H 20 FVL X | 20% glass fiber polypropylene. Heat stabilized. | 8 g/10' | - | 3900 Mpa | - | 7,4 KJ/m2 | - | Classe HB YC | |
Isoglass® H 25 CGF C UV | 25% chemically coupled glass fibre reinforced Polypropylene. Antistatic.UV stabilized. | 6 g/10' | - | 5400 Mpa | - | 11 KJ/m2 | - | Classe HB | |
Isoglass® H 30 CGF 140.80 | 30% glass fiber reinforced homopolymer polypropylene. Compliant to MS-55246 PP140.80. Heat stabilized. | 18 g/10' | - | 5700 Mpa | - | 9 KJ/m2 | - | Classe HB | |
Isoglass® H 30 CGF C | 30% chemically coupled glass fiber reinforced polypropylene. Heat stabilized. | 5 g/10' | - | 6000 Mpa | - | 9 KJ/m2 | - | Classe HB | |
Isoglass® H 30 CGF C UV | 30% chemically coupled glass fiber reinforced polypropylene. Low odor and emission. Compliant to VW44045-PP10 and VW50180. UV stabilized. Heat stabilized. | 5 g/10' | - | 5800 Mpa | - | 9 KJ/m2 | - | Classe HB | |
Isoglass® H 30 CGF F UV | 30% glass fiber reinforced homopolymer polypropylene. UV stabilized. | 13 g/10' | - | 5000 Mpa | - | 8 KJ/m2 | - | Classe HB | |
Isoglass® H 30 CGF S HS | 30% glass fiber reinforced homopolymer polypropylene. Heat stabilized. | 5 kg/10' | - | 6000 Mpa | - | 10 KJ/m2 | - | Classe HB | |
Isoglass® H 30 CGF X HS | 30% chemically coupled glass fiber reinforced polypropylene. Heat stabilized. | 8 g/10' | - | 6000 Mpa | - | 10 KJ/m2 | - | Classe HB | |
Isoglass® H 30 FVL C | PP homo 30% glass fiber. Heat stabilized. | 6 g/10' | - | 5800 MPa | - | 11,5 Kj/m2 | - | Classe HB YC | |
Isoglass® H 30 FVL V | 30% glass fiber filled homopolymer polypropylene. | 20 g/10' | - | 5700 Mpa | - | 10 KJ/m2 | - | Classe HB YC | |
Isoglass® H 30 GFT3 C HS | 30% glass fiber and talc filled polypropylene. Compliant to MS-55246 PP130.50. Heat stabilized. | 8 g/10' | - | 4500 Mpa | - | 7 KJ/m2 | - | Classe HB | |
Isoglass® H 40 CGF C | 40% glass fiber reinforced homopolymer polypropylene. | 7 g/10' | - | 7600 MPa | - | 9 Kj/m2 | - | Classe HB | |
Isoglass® H3V 6009D | 30% talc filled and glass fiber reinforced polypropylene homopolymer. Heat stabilized. Detergent resistant. | 17 g/10' | - | 4700 Mpa | - | 5 KJ/m2 | - | Classe HB YC | |
Isoglass® HGV 6002D | 30% glass fiber homopolymer polypropylene. Heat stabilized. Detergent Resistant. | 17 g/10' | - | 5600 Mpa | - | 9,1 KJ/m2 | - | Classe HB YC | |
Isoglass® HGV 6003X | 30% chemically coupled glass fiber reinforced polypropylene. High flowability. UV stabilized. Chemical Resistant. | 20 g/10' | - | 5500 Mpa | - | 9 KJ/m2 | - | Classe HB | |
Isoglass® K 20 CGF X | 20% glass fiber reinforced copolymer polypropylene. | 10 g/10' | - | 3400 Mpa | - | 13 KJ/m2 | - | Classe HB | |
Isoglass® K 30 CGF X | 30% glass fiber reinforced copolymer polypropylene. | 8 g/10' | - | 4000 Mpa | - | 16 KJ/m2 | - | Classe HB | |
Isoglass® K 40 CGF C | 40% glass fiber reinforced copolymer polypropylene. | 4 g/10' | - | 6200 MPa | - | 15 Kj/m2 | - | Classe HB | |
Isoglass® SC 6029X | 30% chemically coupled glass fiber reinforced copolymer polypropylene. UV stabilized. Heat stabilized. | 5 g/10' | - | 4500 Mpa | - | 22 KJ/m2 | - | Classe HB | |
Isoglass® ST 8020N | 40% chemically coupled glass fiber reinforced polypropylene homopolymer. UV stabilized. Heat stabilized. | 4 g/10' | - | 8000 Mpa | - | 10 KJ/m2 | - | Classe HB | |
Isoglass® SX 4010H | 20% chemically coupled glass fiber reinforced homopolymer polypropylene. Compliant to Renault-Nissan AS8. Heat stabilized. | 10 g/10' | - | 4000 Mpa | - | 8 KJ/m2 | - | Classe HB | |
Isoglass® SX 4015X | 20% chemically coupled glass fiber reinforced homopolymer polypropylene. Compliant to VW 44045. UV stabilized. Heat stabilized. | 8 g/10' | - | 3800 Mpa | - | 6 KJ/m2 | - | Classe HB | |
Isoglass® SX 8022H | 40% chemically coupled glass fiber reinforced polypropylene homopolymer. Heat stabilized. | 10 g/10' | - | 7700 Mpa | - | 10 KJ/m2 | - | Classe HB | |
Isoglass® XX 6014D | 30% chemically coupled glass fiber reinforced polypropylene, high stiffness. Heat stabilized. | 8 g/10' | - | 7000 Mpa | - | 9 KJ/m2 | - | Classe HB |
Isoglass® XT
Hochleistungs-Polypropylen mit chemisch gekoppelten Glasfasern. Die von dieser PPGF-Reihe garantierten Eigenschaften orientieren sich an denen von Hochleistungspolymeren, wobei jedoch die Eigenschaften von PP garantiert werden. Diese Produkte bieten eine gute Kombination aus Wärmebeständigkeit und mechanischer Festigkeit in Verbindung mit hoher Steifigkeit.Name | Compound | MFR ISO 1133 | MFR (g/10’) ASTM D1238 | Biegemodul ISO 178 | MFR (g/10’) ASTM D1238 | Izod Gekerbt ISO 180/1A | Izod Gekerbt ASTM D256 | Entflammbarkeit UL94/2 | |
---|---|---|---|---|---|---|---|---|---|
Isoglass® XT 1003H | 50% chemically coupled high performance glass fiber reinforced polypropylene homopolymer. High stiffness grade. Heat stabilized. | 3,5 g/10' | - | 13000 Mpa | - | 9 KJ/m2 | - | Classe HB | |
Isoglass® XT 4001D | 20% chemically coupled glass fiber reinforced polypropylene. | 7 g/10' | - | 4000 Mpa | - | 7 KJ/m2 | - | Classe HB YC | |
Isoglass® XT 4007U | 20% chemically coupled high performance reinforced polypropylene homopolymer. High stiffness and low emission. Compliant to DBL 5430. UV stabilized. | 7 g/10' | - | 6100 Mpa | - | 9 KJ/m2 | - | Classe HB | |
Isoglass® XT 6001D | 30% chemically coupled high performance glass fiber reinforced polypropylene compound. | 5 g/10' | - | 6800 Mpa | - | 11 KJ/m2 | - | Classe HB YC | |
Isoglass® XT 6001H | 30% chemically coupled high performance glass fiber reinforced polypropylene. Heat stabilized. | 3,5 g/10' | - | 6500 Mpa | - | 10 KJ/m2 | - | Classe HB | |
Isoglass® XT 6010H | 30% chemically coupled high performance glass fiber reinforced polypropylene homopolymer. High stiffness and low emission. | 6 g/10' | - | 8400 Mpa | - | 10 KJ/m2 | - | Classe HB | |
Isoglass® XT 7001H | 35% chemically coupled glass fiber reinforced polypropylene homopolymer. Low flowability grade. Heat stabilized. | 3 g/10' | - | 8000 Mpa | - | 12 KJ/m2 | - | Classe HB | |
Isoglass® XT 8008H | 40% chemically coupled high performance glass fiber reinforced polypropylene homopolymer. High stiffness and low emission. | 5 g/10' | - | 10000 Mpa | - | 10 KJ/m2 | - | Classe HB |
Isoglass® LFT
Polypropylen-Pultrusionscompound mit langen Fasern für Anwendungen mit hoher Dimensionsstabilität und hoher thermischer und mechanischer Performance. Der Einsatz von PP LFT ist vor allem bei konstruktiven Anwendungen gefragt, bei denen die Orientierung der langen Fasern den anisotropen Effekt modifiziert, wodurch die Dimensionsstabilität erhöht und Anwendungen mit sehr hoher Steifigkeit erreicht werden. Die Produktpalette ist mit verschiedenen Fasergehalten erhältlich, auch mit hohen Konzentrationen.Name | Compound | MFR ISO 1133 | MFR (g/10’) ASTM D1238 | Biegemodul ISO 178 | MFR (g/10’) ASTM D1238 | Izod Gekerbt ISO 180/1A | Izod Gekerbt ASTM D256 | Entflammbarkeit UL94/2 | |
---|---|---|---|---|---|---|---|---|---|
Isoglass® LFT 1001H | PP homo 50% long glass fiber, heat stabilized. | / | - | 10500 MPa | - | 29 Kj/m2 | - | Classe HB | |
Isoglass® LFT LFT 0603H | 30% chemically coupled long glass fiber reinforced polypropylene compound with very high mechanical properties and heat stabilized. | / | - | 6300 Mpa | - | 21 Kj/m2 | - | Classe HB |
Green Isofil®
Polypropylen-Verbundwerkstoff mit mineralischen Füllstoffen, der Anteile an Post-Industrie- oder Post-Consumer-Recyclingmaterial enthält. Die Produkte entsprechen den kürzlich von der Automotive- und Haushaltsgeräteindustrie eingeführt Standards.Name | Compound | MFR ISO 1133 | MFR (g/10’) ASTM D1238 | Biegemodul ISO 178 | MFR (g/10’) ASTM D1238 | Izod Gekerbt ISO 180/1A | Izod Gekerbt ASTM D256 | Entflammbarkeit UL94/2 | |
---|---|---|---|---|---|---|---|---|---|
Green Isofil® HK 40 C F | PP copo 40% calcium carbonate, heat stabilized, detergent resistant. | 20 g/10' | - | 1900 MPa | - | 3,3 Kj/m2 | - | Classe HB | |
Green Isofil® K 30 T T HS | 30% talc filled polypropylene copolymer. Industrial quality. Heat stabilized. | 3 g/10' | - | 2200 MPa | - | 6 Kj/m2 | - | Classe HB |
Green Isoglass®
Glasfaserverstärktes Polypropylen unter teilweiser Verwendung von Rohstoffen, die aus Industrie- und Post-Consumer-Quellen stammen. Die Produkte sind in Übereinstimmung mit einigen kürzlich von der Automobil- und Haushaltsgerätebranche eingeführten Normen erhältlich.Name | Compound | MFR ISO 1133 | MFR (g/10’) ASTM D1238 | Biegemodul ISO 178 | MFR (g/10’) ASTM D1238 | Izod Gekerbt ISO 180/1A | Izod Gekerbt ASTM D256 | Entflammbarkeit UL94/2 | |
---|---|---|---|---|---|---|---|---|---|
Green Isoglass® H 30 CGF C HS | 30% chemically coupled glass fiber reinforced polypropylene with 30% circular polymer source. Heat stabilized. | 6 g/10' | - | 4900 MPa | - | 9 Kj/m2 | - | Classe HB | |
Green Isoglass® H 40 CGF X HS | 40% glass fiber reinforced polypropylene. Industrial quality. Heat stabilized. | 10 g/10' | - | 6000 MPa | - | 9 Kj/m2 | - | Classe HB |